ABS ER875 KUMHO KOREA
259
Form:Granules | Grade:Injection grade
Properties:
Low temperature resistanc
Typical Applications:
Food packagingHome appliance components
Product Description
Certificates(1)
Datasheet
Product Description
| Typical Applications: | Food packaging | Home appliance components |
| Properties: | Low temperature resistanc |
Certificates

Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | 3.20mm | ASTM D256 | 350 | J/m |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | UL 94 | HB | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| bending strength | ASTM D790 | 72.0 | Mpa | |
| tensile strength | ASTM D638 | 47.0 | Mpa | |
| elongation | Break | ASTM D638 | 35 | % |
| Bending modulus | ASTM D790 | 2300 | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 1.8MPa,Unannealed | ASTM D648 | 85.0 | °C |
| Vicat softening temperature | ASTM D15252 | 96.0 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | ASTM D792 | 1.04 | g/cm³ | |
| melt mass-flow rate | 220°C/10.0kg | ASTM D1238 | 25 | g/10min |
| Shrinkage rate | MD | ASTM D955 | 0.30-0.60 | % |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Surface resistivity | IEC 60093 | >1.0E+14 | ohms | |
| Volume resistivity | IEC 60093 | >1.0E+14 | ohms·cm | |
| Supplementary Information | Test Condition | Test Method | Test Result | Test Unit |
| CSAFileNo | LS66457 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.