Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ASTMD3575 | 0.0481 g/cm³ | |
VOCContent | 11 % | ||
0.30 % | |||
0.800到1.70 mm |
Supplementary Information | Test Condition | Test Method | Test Result |
---|---|---|---|
Tear strength - atMaximmLoad | ASTMD3575 | 3.9 kN/m |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
compressive strength | ASTMD3575 | 0.341 MPa | |
tensile strength | Break | ASTMD3575 | 0.645 MPa |
bending strength | ASTMC203 | 0.600 MPa | |
ASTMC203 | 0.656 MPa | ||
compressive strength | ASTMD3575 | 0.299 MPa | |
ASTMD3575 | 0.418 MPa | ||
ASTMD3575 | 0.811 MPa | ||
Bending Strain | ASTMC203 | 9.4 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.
Contact Us
Get App
Top