PA66 FR70M30 VO NC010 DUPONT USA
85
Form:Granules | Grade:Flame retardant grade
Properties:
Mineral reinforcementFlame retardant
Typical Applications:
Industrial applicationsIndustrial machineryElectronic fieldElectrical field
Product Description
Certificates(1)
Datasheet
Product Description
| Typical Applications: | Industrial applications | Industrial machinery | Electronic field | Electrical field |
| Properties: | Mineral reinforcement | Flame retardant |
Certificates

Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 20 | kJ/m² |
| -30°C | ISO 179/1eU | 20 | kJ/m² | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| FMVSS flammability | FMVSS302 | DNI | ||
| Extreme Oxygen Index | ISO 4589-2 | 40 | % | |
| UL flame retardant rating | 0.75mm | IEC 60695-11-10,-20 | V-2 | |
| 1.5mm | IEC 60695-11-10,-20 | V-0 | ||
| 1.5mm | UL 94 | V-0 | ||
| 0.75mm | UL 94 | V-2 | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile strain | Break | ISO 527-2 | 2.0 | % |
| tensile strength | Break | ISO 527-2 | 65.0 | Mpa |
| Tensile modulus | ISO 527-2 | 6200 | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Melting temperature | ISO 11357-3 | 263 | °C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 145 | °C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Top out temperature | 210 | °C | ||
| Shrinkage rate | MD | ISO 294-4 | 0.80 | % |
| TD | ISO 294-4 | 0.90 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.