PCTG Tritan™ MX731 EASTMAN USA
129
- Properties:Easy to processheat-resisting
- Usages:Household daily necessitiElectrical applications
Technical Data Sheet
物理性能 | Test Condition | Test Method | Test Result |
---|---|---|---|
收缩率 | MD | ASTMD955 | 0.50to0.70 % |
热性能 | Test Condition | Test Method | Test Result |
---|---|---|---|
热变形温度 | 0.45MPa,未退火 | ASTMD648 | 94.0 °C |
1.8MPa,未退火 | ASTMD648 | 80.0 °C |
光学性能 | Test Condition | Test Method | Test Result |
---|---|---|---|
透射率 | 总计 | ASTMD1003 | 91.0 % |
雾度 | ASTMD1003 | <1.0 % |
机械性能 | Test Condition | Test Method | Test Result |
---|---|---|---|
伸长率 | 断裂,23°C | ASTMD638 | 210 % |
拉伸应变 | 断裂,23°C | ISO527-2 | 150 % |
弯曲模量 | 23°C | ASTMD790 | 1580 Mpa |
23°C | ISO178 | 1500 Mpa | |
弯曲应力 | 23°C | ISO178 | 60.0 Mpa |
弯曲强度 | 屈服,23°C | ASTMD790 | 64.0 Mpa |
拉伸模量 | 23°C | ASTMD638 | 1580 Mpa |
23°C | ISO527-2 | 1600 Mpa | |
抗张强度 | 屈服,23°C | ASTMD638 | 43.0 Mpa |
拉伸应力 | 屈服,23°C | ISO527-2 | 44.0 Mpa |
抗张强度 | 断裂,23°C | ASTMD638 | 52.0 Mpa |
拉伸应力 | 断裂,23°C | ISO527-2 | 49.0 Mpa |
伸长率 | 屈服,23°C | ASTMD638 | 7.0 % |
拉伸应变 | 屈服,23°C | ISO527-2 | 7.0 % |
硬度 | Test Condition | Test Method | Test Result |
---|---|---|---|
洛氏硬度 | R计秤,23°C | ASTMD785 | 111 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.