PUR-Ether/MDI Andur M-11 (1,4BD) USA Anderson Development
Product Description
Certificates(0)
Datasheet
Product Description
Certificates
No Data...
Technical Data Sheet
| elastomer | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| elongation | Break | ASTM D412 | 450 | % |
| Permanent compression deformation | ASTM D395 | 33 | % | |
| Shore hardness | ASTM D2632 | 28 | % | |
| tensile strength | 300%Strain | ASTM D412 | 26.2 | MPa |
| Yield | ASTM D412 | 51.7 | MPa | |
| 100%Strain | ASTM D412 | 10.3 | MPa | |
| 200%Strain | ASTM D412 | 17.2 | MPa | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| compressive strength | 20%Strain | ASTM D695 | 6.89 | MPa |
| 25%Strain | ASTM D695 | 8.96 | MPa | |
| 50%Strain | ASTM D695 | 27.6 | MPa | |
| Taber abraser | ASTM D1044 | 28.1 | mg | |
| compressive strength | 2%Strain | ASTM D695 | 1.03 | MPa |
| 5%Strain | ASTM D695 | 2.41 | MPa | |
| 10%Strain | ASTM D695 | 4.14 | MPa | |
| 15%Strain | ASTM D695 | 5.52 | MPa | |
| thermosetting | Test Condition | Test Method | Test Result | Test Unit |
| storage stability | 4.0to7.0 | min | ||
| stripping time | 35 | min | ||
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Shore hardness | ShoreD | ASTM D2240 | 43 | |
| ShoreA | ASTM D2240 | 95 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.