Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | | 1.65 g/cm3 |
Other performance | Test Condition | Test Method | Test Result |
---|
RTI Str | | 2.0mm | 130 ℃ |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
tensile strength | | 23℃ | 113 MPa |
| Test Condition | Test Method | Test Result |
---|
Rockwell hardness | | | 79 |
Glass Transition Temperature | | | 176 ℃ |
Flame retardancy | | 2.0mm | V-0 |
Flame retardancy | | 2.0mm | V-0 |
RTI Imp | | 2.0mm | 130 ℃ |
IZOD notch impact strength | | 23℃ | 28.8 J/m |
tensile elongation | | 断裂,23℃ | 1.0 % |
Flexural modulus | | 23℃ | 13000 MPa |
bending strength | | 23℃ | 176 MPa |
RTI Elec | | 2.0mm | 130 ℃ |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | 1.8MPa,未退火 | 160 ℃ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.