PA66 3010N5 MITSUBISHI ENGINEERING JAPAN
66
Form:Granules | Grade:Injection grade
Properties:
Low temperature resistancwear resistantNon halogen flame retarda
Typical Applications:
Automotive componentsElectronic and electrical components
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Automotive components | Electronic and electrical components |
| Properties: | Low temperature resistanc | wear resistant | Non halogen flame retarda |
Certificates
No Data...
Technical Data Sheet
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | ISO 179 | 3(7) | KJ/m | |
| ISO 179 | 111 | KJ/m | ||
| elongation | Break | 3.2 | % | |
| Fracture stress | 80 | Mpa | ||
| Bending modulus | D178 | 3600(1900) | Mpa | |
| bending strength | D178 | 133(64) | Mpa | |
| Tensile modulus | ISO 527-1 | 3500/2100 | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | UL 94 | V-0 | ||
| Hot deformation temperature | HDT | D648 | 80(231) | °C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Shrinkage rate | 1.5 | TD% | ||
| 1.3 | MD% | |||
| Water absorption rate | D570 | 2.7 | % | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Compared to the Leakage Traceability Index (CTI) | IEC 112 | >600 | ||
| Dielectric loss | IEC 250 | 0.008(0.019) | ||
| Dielectric constant | D150 | 4 | Pf/m | |
| Dielectric strength | IEC 243-1 | 26 | MV/m |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.