HDPE PONACOM PE 4410-2 Ponachem Compound GmbH
0
Technical Data Sheet
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Oxygen induction time | 200°C | ISO 868 | >20 min |
| Melting temperature | ISO 3146 | 134 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| melt mass-flow rate | VolatileMatter-1hr(105°C) | ISO 1133 | <0.035 % |
| Apparent density | ISO 60 | 0.46 g/cm³ | |
| density | ISO 1183 | 0.950to0.953 g/cm³ | |
| melt mass-flow rate | 炭黑含量 | ISO 1133 | >2.0 % |
| 200°C/21.6kg | ISO 1133 | 20to24 g/10min | |
| 190°C/5.0kg | ISO 1133 | 0.80to1.2 g/10min | |
| 190°C/2.16kg | ISO 1133 | 0.30to0.40 g/10min |
| hardness | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Shore hardness | ShoreD | ISO 868 | 56to60 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.