LLDPE K203 Chevron Phillips
0
- Properties:Good processing performance excellent melt strength good flexibility excellent stress cracking resistance
- Usages:Application of Hats and Geomembranes
Technical Data Sheet
| Basic Performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| density | ASTM D-1505 | 0.924 g/cc | |
| melt mass-flow rate | 190℃/21.6kg | ASTM D-1238 | 15 g/10min |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Environmental stress cracking resistance | 50℃ | ASTM D-1693 | ≥1500 hour |
| tensile strength | Yield | ASTM D-638 | 13 MPa |
| elongation | Break | ASTM D-638 | ≥700 % |
| Bending modulus | ASTM D-790 | 0.480 GPa |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Processing temperature | 193-232 ℃ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.