PA6/ABS 1120 A4 GF8 USA TPC

0
  • Properties:
    Filler reinforcement material glass fiber reinforcement material appearance available colors
  • Compare

Technical Data Sheet

flammabilityTest ConditionTest MethodTest Result
UL flame retardant rating3.18 mmUL 94HB
mechanical propertiesTest ConditionTest MethodTest Result
Impact strength of cantilever beam gap23°C, 3.18 mmASTM D256110 J/m
bending strengthASTM D79077.9 MPa
Bending modulusASTM D7902760 MPa
elongationBreakASTM D6385.0 %
tensile strengthBreakASTM D63851.0 MPa
Rockwell hardnessR-ScaleASTM D785108
thermal performanceTest ConditionTest MethodTest Result
Hot deformation temperature1.8 MPa, UnannealedASTM D64887.8 °C
Hot deformation temperature0.45 MPa, UnannealedASTM D648107 °C
Physical propertiesTest ConditionTest MethodTest Result
Shrinkage rateMD (3.18 mm)ASTM D9550.40 %
densityASTM D7921.12 g/cm³
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.