PS Generic PPE+PS+Nylon Generic
Product Description
Certificates(0)
Datasheet
Product Description
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179 | 11to55 | kJ/m² |
| Impact strength of cantilever beam gap | 23°C | ASTM D256 | 73to680 | J/m |
| 23°C | ISO 180 | 9.5to55 | kJ/m² | |
| Dart impact | 23°C | ASTM D3763 | 4.00to60.0 | J |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| tensile strength | Yield,23°C | ISO 527-2 | 50.0to65.2 | MPa |
| Break,23°C | ASTM D638 | 49.8to60.2 | MPa | |
| elongation | Yield,23°C | ASTM D638 | 4.7to5.0 | % |
| Yield,23°C | ISO 527-2 | 3.5to5.1 | % | |
| Break,23°C | ASTM D638 | 2.2to100 | % | |
| Break,23°C | ISO 527-2 | 2.8to51 | % | |
| Bending modulus | 23°C | ASTM D790 | 1840to2730 | MPa |
| 23°C | ISO 178 | 1860to2850 | MPa | |
| bending strength | 23°C | ASTM D790 | 73.5to85.7 | MPa |
| 23°C | ISO 178 | 70.0to103 | MPa | |
| Yield,23°C | ASTM D790 | 74.7to99.3 | MPa | |
| tensile strength | Break,23°C | ISO 527-2 | 45.0to55.5 | MPa |
| Tensile modulus | 23°C | ASTM D638 | 1820to3320 | MPa |
| 23°C | ISO 527-2 | 2000to3050 | MPa | |
| tensile strength | Yield,23°C | ASTM D638 | 53.5to65.6 | MPa |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | TD | ASTME831 | 5.9E-5到1.0E-4 | cm/cm/°C |
| TD | ISO 11359-2 | 8.9E-5到9.1E-5 | cm/cm/°C | |
| thermal conductivity | 23°C | ISO 8302 | 0.23to0.24 | W/m/K |
| Hot deformation temperature | 0.45MPa,Unannealed | ASTM D648 | 154to196 | °C |
| 0.45MPa,Unannealed | ISO 75-2/B | 174to193 | °C | |
| 1.8MPa,Unannealed | ASTM D648 | 83.9to197 | °C | |
| Vicat softening temperature | -- | ASTM D1525 | 178to233 | °C |
| -- | ISO 306 | 169to246 | °C | |
| Linear coefficient of thermal expansion | MD | ASTME831 | 7.5E-5到9.8E-5 | cm/cm/°C |
| MD | ISO 11359-2 | 8.0E-5到1.0E-4 | cm/cm/°C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | -- | ASTM D792 | 1.07to1.12 | g/cm³ |
| 23°C | ISO 1183 | 1.07to1.25 | g/cm³ | |
| melt mass-flow rate | 280°C/5.0kg | ASTM D1238 | 8.0to21 | g/10min |
| Melt Volume Flow Rate (MVR) | 280°C/5.0kg | ISO 1133 | 7.50to19.0 | cm³/10min |
| Shrinkage rate | MD:23°C | ASTM D955 | 1.2to1.8 | % |
| TD:23°C | ASTM D955 | 1.1to1.3 | % | |
| Water absorption rate | 23°C,24hr | ASTM D570 | 0.39to0.60 | % |
| Saturation,23°C | ISO 62 | 3.5to4.2 | % | |
| Equilibrium,23°C,50%RH | ISO 62 | 1.2 | % | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Volume resistivity | 23°C | ASTM D257 | 4.0E+3到1.1E+15 | ohms·cm |
| Relative permittivity | 23°C | IEC 60250 | 3.17 | |
| Dissipation factor | 23°C | IEC 60250 | 0.024to0.072 | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Ball Pressure Test | ISO 2039-1 | 75.0to90.0 | MPa |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.