Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | 23°C | ISO 180/1C | NoBreak | |
| 23°C | ISO 180/A | 50 | kJ/m² | |
| -20°C | ISO 180/A | 40 | kJ/m² | |
| -30°C | ISO 180/1C | NoBreak | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Nominal tensile fracture strain | 23°C | ISO 527-2/50 | >50 | % |
| Tensile strain | Yield,23°C | ISO 527-2/50 | 5.0 | % |
| tensile strength | Break,23°C | ISO 527-2/50 | 50.0 | Mpa |
| Yield,23°C | ISO 527-2/50 | 55.0 | Mpa | |
| Tensile modulus | 23°C | ISO 527-2/1 | 2250 | Mpa |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Vicat softening temperature | ISO 306/B120 | 140 | °C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 110 | °C |
| 0.45MPa,Unannealed | ISO 75-2/B | 125 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Shrinkage rate | MD:90°C,1hr | ISO 2577 | 0.10-0.20 | % |
| MD2 | ISO 2577 | 0.60-0.80 | % | |
| TD:90°C,1hr | ISO 2577 | 0.10-0.20 | % | |
| TD2 | ISO 2577 | 0.60-0.80 | % | |
| Melt Volume Flow Rate (MVR) | 265°C/5.0kg | ISO 1133 | 22.0 | cm3/10min |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.