PC FR6005 013617 COVESTRO SHANGHAI
158
Form:Granules | Grade:Flame retardant grade
Properties:
Good appearanceImpact improvementEasy to demould
Typical Applications:
Electronic and electrical enclosure
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Electronic and electrical enclosure |
| Properties: | Good appearance | Impact improvement | Easy to demould |
Certificates
No Data...
Technical Data Sheet
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Puncture resistance | -30℃ | ISO 6603 | 55 | J |
| 23℃ | ISO 6603 | 54 | J | |
| Maximum puncture resistance -30 ° C | ISO 6603 | 6100 | N | |
| Maximum puncture resistance at 23 ° C | ISO 6603 | 5100 | N | |
| Impact strength of cantilever beam gap | 23°C | ISO 179 | 20 | kJ/m² |
| 23°C | ISO 179 | 50 | kJ/m² | |
| 23°C | ISO 179 | 68 | kJ/m² | |
| 23°C | ISO 180 | 15 | kJ/m² | |
| 23°C | ISO 180 | 50 | kJ/m² | |
| 23°C | ISO 180 | 60 | kJ/m² | |
| Bending modulus | 2.0mm/min | ISO 178 | 2400 | Mpa |
| bending strength | 2.0mm/min | ISO 178 | 90 | Mpa |
| Elongation at Break | 50mm/min | ISO 527 | 135 | % |
| 50mm/min | ISO 527 | 50 | % | |
| elongation | Yield,50mm/min | ISO 527 | 6 | % |
| tensile strength | Break50mm/min | ISO 527 | 66 | Mpa |
| Yield,50mm/min | ISO 527 | 62 | Mpa | |
| Tensile modulus | 0mm/min | ISO 527 | 2300 | Mpa |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Vicat softening temperature | 50°C/hr50N | ISO 306 | 142 | °C |
| 120°C/hr50N | ISO 306 | 144 | °C | |
| Hot deformation temperature | 0.45MPa | ISO 75 | 136 | °C |
| 1.8MPa | ISO 75 | 121 | °C | |
| Linear coefficient of thermal expansion | Flow, 23~55℃ | ISO 11359 | 0.000070 | cm/cm/°C |
| 垂直, 23~55℃ | ISO 11359 | 0.000070 | cm/cm/°C | |
| Ball indentation test | ISO 11359-2 | 134 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| melt mass-flow rate | 300°C1.2kg | ISO 1133 | 9 | cm3/10min |
| Shrinkage rate | ISO 2577 | 0.6-0.8 | % | |
| Flow | ISO 2577 | 0.6-0.8 | % | |
| density | ISO 1183 | 1200 | kg/m3 | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Volume resistivity | IEC 60093 | 90000000000000000 | Ω.m | |
| Surface resistivity | IEC 60093 | 400000000000000000 | Ω | |
| CTI solution A | IEC 60112 | 200 | V | |
| flame retardant performance | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 0.75mm | UL 94 | V-2 | |
| 1.0mm | UL 94 | V-0 | ||
| 1.2mm | UL 94 | V-0 | ||
| 1.2mm | UL 94 | V-1 | ||
| 1.5mm | UL 94 | V-0 | ||
| 3.0mm | UL 94 | V-0 | ||
| Glow wire ignition temperature (GWIT) | 1.0mm | ISO 11359-2 | 875 | °C |
| 1.5mm | ISO 11359-2 | 850 | °C | |
| 3.0mm | ISO 11359-2 | 900 | °C | |
| Relative temperature of heating wire | 1.0mm | ISO 11359-2 | 850 | °C |
| 1.5mm | ISO 11359-2 | 960 | °C | |
| 3.0mm | ISO 11359-2 | 960 | °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.