Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ASTMD792 | 0.987到1.03 g/cm³ | |
melt mass-flow rate | ASTMD1238 | 11到16 g/10min | |
Shrinkage rate | ASTMD955 | 0.65到1.0 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
tensile strength | ISO527-2 | 33.9到44.6 MPa | |
ASTMD638 | 27.6到41.5 MPa | ||
elongation | ASTMD638 | 6.5到15 % | |
ASTMD638 | 83到200 % | ||
ISO527-2 | 46到120 % | ||
Flexural modulus | ASTMD790 | 1340到1560 MPa | |
bending strength | ASTMD790 | 49.0到53.2 MPa | |
Tensile modulus | ASTMD638 | 1170到1710 MPa | |
ISO527-2 | 1660到1760 MPa | ||
tensile strength | ASTMD638 | 33.8到43.8 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|---|---|---|
Impact strength of cantilever beam gap | ASTMD256 | 150到590 J/m | |
Dart impact equipped with measuring instruments | ASTMD3763 | 36.2到45.9 J |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
ASTMD648 | 110到113 °C | ||
ASTMD648 | 71.1到92.0 °C | ||
vicat | ASTMD1525 | 85.0到146 °C | |
ISO306 | 102到118 °C | ||
ASTME831 | 8.1E-5到1.6E-4 cm/cm/°C | ||
ASTME831 | 7.2E-5到1.1E-4 cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.