Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD792 | 1.32到1.36 g/cm³ |
thermosetting | Test Condition | Test Method | Test Result |
---|
| | | 按重量计算的混合比:100按容量计算的混合比:4.0 |
| | | 按重量计算的混合比:17按容量计算的混合比:1.0 |
| | | 40到50 min |
Thermosetting mixed viscosity | | ASTMD2393 | 1000到2000 cP |
hardness | Test Condition | Test Method | Test Result |
---|
| | ASTMD2240 | 50到65 |
Electrical performance | Test Condition | Test Method | Test Result |
---|
Dissipation Factor | | ASTMD150 | 0.010到0.011 |
Volume resistivity | | ASTMD257 | 2.7E+12到2.8E+12 ohms·cm |
dielectric strength | | ASTMD149 | 17到20 kV/mm |
dielectric constant | | ASTMD2520 | 3.20到3.28 |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Glass Transition Temperature | | ASTME1356 | -55.0 °C |
| | ASTMD696 | 3.5E-4到3.7E-4 cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.