Technical Data Sheet
Cured Properties | Test Condition | Test Method | Test Result |
---|
Supporting hardness | | | 54到62 |
Supporting hardness | | | 56到64 |
Supporting hardness | | | 66到74 |
tensile strength | | ASTMD412 | 5.00到5.69 MPa |
elongation | Break | ASTMD412 | 130到180 % |
tear strength | | ASTMD624 | 10.5到14.0 kN/m |
electric strength | | | 20 kV/mm |
| | | 2.90 |
Volume resistivity | | | 5E+14 ohms·cm |
Dissipation Factor | | | 0.015 |
Coverage-Cured | | | 0.748 cm³/g |
thermosetting | Test Condition | Test Method | Test Result |
---|
| Resin | | 按容量计算的混合比:100按重量计算的混合比:10 |
| Hardener | | 按容量计算的混合比:14按重量计算的混合比:1.0 |
| Shelf Life | | 26 wk |
| | | 90000到110000 cP |
Uncured Properties | Test Condition | Test Method | Test Result |
---|
colour | | | Green |
colour | | | Tan |
| | | 1.0到2.0 Pa·s |
| | | 140到160 Pa·s |
| | | 16到24 hr |
| Pot Life | | 60到120 min |
physical property | Test Condition | Test Method | Test Result |
---|
density | | | 1.34 g/cm³ |
Thermal performance | Test Condition | Test Method | Test Result |
---|
ServiceTemperature-Cured | | | -51到343 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.