Technical Data Sheet
thermosetting | Test Condition | Test Method | Test Result |
---|---|---|---|
Hardener | 按容量计算的混合比:1.0按重量计算的混合比:18 | ||
200到270 min | |||
52 wk | |||
Thermosetting mixed viscosity | ASTMD2393 | 24000 cP | |
stripping time | 7200到10000 min | ||
Resin | 按容量计算的混合比:3.2按重量计算的混合比:100 |
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
Apparent density | ASTMD1895 | 1.47 g/cm³ | |
Shrinkage rate | ASTMD955 | 0.050 % |
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
ASTMD2240 | 90 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile modulus | ASTMD638 | 4070 MPa | |
tensile strength | Break | ASTMD638 | 40.2 MPa |
elongation | Yield | ASTMD638 | 2.3 % |
Flexural modulus | ASTMD790 | 2760 MPa | |
compressive strength | ASTMD695 | 71.4 MPa |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.