PP 1101S

0
  • Properties:
    Fiber grade
  • Usages:
    High speed spinning of low denier synthetic fibers

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
melt mass-flow rateGB/T 3682-200024.1 g/10min
isotactic indexGB/T 2412-200898.6 %
Granular ash content (mass fraction)GB/T 9345.1-2008195 mg/kg
Mechanical propertiesTest ConditionTest MethodTest Result
tensile yield stressGB/T 1040.2-200634.7 MPa
Tensile modulus of elasticityGB/T 1040.2-20061570 MPa
Tensile fracture stressGB/T 1040.2-200623.1 MPa
Tensile fracture nominal strainGB/T 1040.2-2006390 %
Impact of simply supported beam gap(GB/T 1043.1-20082.9 kJ/m2
Thermal performanceTest ConditionTest MethodTest Result
yellow indexHG/T 3862-2006-1.3
fish eyeGB/T 6595-19860 个/1520㎡
fish eye1个/1520㎡
Particle appearanceTest ConditionTest MethodTest Result
saladSH/T 1541-20060 个/kg
black kernelSH/T 1541-20060 个/kg
Large and small particlesSH/T 1541-20061.3 g/kg
SH/T 1541-200629 个/kg
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.