EAA ESCOR™  5050 EXXONMOBIL USA

58

Technical Data Sheet

Basic PerformanceTest ConditionTest MethodTest Result
densityASTM D-4703/D-15050.936 g/m3
melt mass-flow rateASTM D-12388.4 g/10min
thermal performanceTest ConditionTest MethodTest Result
Vicat softening temperatureASTM D-152577 °C
Maximum melting temperatureASTM D-341897 °C
Physical propertiesTest ConditionTest MethodTest Result
Acrylic acid contentExxonMobil Method9 %wt
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.