physical property Test ConditionTest MethodTest Result
densityISO 11831.42 g/cm³
melt mass-flow rateISO 11332.0 g/10min
Shrinkage rate1.8to2.2 %
Water absorption rateISO 620.20 %
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strength YieldISO 527-265.0 MPa
Tensile strainYieldISO 527-28.0 %
Tensile strainBreakISO 527-280 %
Tensile modulusISO 527-23000 MPa
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapISO 180/A60 kJ/m²
Suspended wall beam without notch impact strengthISO 180无断裂
Electrical performanceTest ConditionTest MethodTest Result
Compared to the Leakage Tracking Index (CTI)IEC 60112PLC 0
Thermal performanceTest ConditionTest MethodTest Result
Heat distortion temperatureISO 75-2/B165 °C
Heat distortion temperatureISO 75-2/A110 °C
Heat distortion temperature80.0 °C
vicatISO 306/A120165 °C
ball-indentation hardnessIEC 60695-10-2通过
melting temperatureDSC175 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.