ASA+PA Romiloy® 3020/07 ROMIRA GERMANY
Properties:
mechanical properties
Product Description
Certificates(0)
Datasheet
Product Description
| Properties: | mechanical properties |
Certificates
No Data...
Technical Data Sheet
| Test Condition | Test Method | Test Result | Test Unit | |
|---|---|---|---|---|
| tensile strength | 23°C | MPa | 37.0 | 34.0 |
| Tensile modulus | 23°C | MPa | 1700 | 1200 |
| Water absorption rate | 23°C,24hr | % | 1.0 | -- |
| Shrinkage rate | 23°C | % | 0.60to0.90 | -- |
| melt mass-flow rate | 260°C/5.0kg | g/10min | 15 | -- |
| density | 23°C | g/cm³ | 1.06 | -- |
| thermal conductivity | W/m/K | 0.25 | -- | |
| Vicat softening temperature | °C | 105 | -- | |
| Hot deformation temperature | 0.45MPa,Unannealed | °C | 89.0 | -- |
| Impact strength of simply supported beam without notch | 23°C | 无断裂 | -- | |
| -30°C | 无断裂 | -- | ||
| Charpy Notched Impact Strength | 23°C | kJ/m² | 60 | -- |
| -30°C | kJ/m² | 11 | -- | |
| bending strength | 23°C | MPa | 58.0 | -- |
| Tensile strain | Break,23°C | % | >100 | >200 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.