PA6 Staramide BG6U EUROSTAR FRANCE
Properties:
Filler glass fiber reinforced material 30% filler by weight
Product Description
Certificates(0)
Datasheet
Product Description
| Properties: | Filler | glass fiber reinforced material | 30% | filler by weight |
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 11 | kJ/m² |
| -20°C | ISO 180/1A | 10 | kJ/m² | |
| -40°C | ISO 180/1A | 9.0 | kJ/m² | |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 90 | kJ/m² |
| -30°C | ISO 179/1eU | 75 | kJ/m² | |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 11 | kJ/m² |
| -30°C | ISO 179/1eA | 9.0 | kJ/m² | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| Extreme Oxygen Index | ISO 4589-2 | 25 | % | |
| Burning wire flammability index | 2.0mm | IEC 60695-2-12 | 650 | °C |
| UL flame retardant rating | 0.75mm | UL 94 | HB | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| bending strength | ISO 178 | 230 | MPa | |
| Bending modulus | ISO 178 | 8000 | MPa | |
| Tensile strain | Break | ISO 527-2/5 | 3.6 | % |
| tensile strength | Break | ISO 527-2/5 | 160 | MPa |
| Tensile modulus | ISO 527-2/1 | 9500 | MPa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| thermal conductivity | ISO 8302 | 0.33 | W/m/K | |
| Linear coefficient of thermal expansion | TD:23to60°C | ISO 11359-2 | 8.5E-05 | cm/cm/°C |
| Hot deformation temperature | 0.45MPa,Unannealed,100mmSpan | ISO 75-2/Be | 220 | °C |
| 1.8MPa,Unannealed,100mmSpan | ISO 75-2/Ae | 210 | °C | |
| Vicat softening temperature | ISO 306/B50 | 215 | °C | |
| Linear coefficient of thermal expansion | MD:23to60°C | ISO 11359-2 | 2.5E-05 | cm/cm/°C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 1.8 | % |
| Saturation,23°C | ISO 62 | 6.5 | % | |
| density | ISO 1183 | 1.36 | g/cm³ | |
| Shrinkage rate | MD | Internal Method | 0.20to0.40 | % |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Dielectric strength | 3.20mm,in Oil | IEC 60243-1 | 20 | kV/mm |
| Volume resistivity | IEC 60093 | >1.0E+16 | ohms·cm | |
| Surface resistivity | IEC 60093 | >1.0E+16 | ohms | |
| Compared to the anti leakage trace index | SolutionB | IEC 60112 | PLC 2 | |
| -- | IEC 60112 | PLC 1 | ||
| Dissipation factor | 1MHz | IEC 60250 | 0.016 | |
| Relative permittivity | 50Hz | IEC 60250 | 3.60 | |
| 60Hz | IEC 60250 | 3.60 | ||
| 1MHz | IEC 60250 | 3.40 | ||
| Dissipation factor | 50Hz | IEC 60250 | 6.1E-03 | |
| 60Hz | IEC 60250 | 6.1E-03 | ||
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Rockwell hardness | L-Sale | ISO 2039-2 | 112 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.