Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD792 | 1.35 g/cm³ |
Water absorption rate | | ASTMD570 | 0.080 % |
Water absorption rate | Saturation | ASTMD570 | 0.50 % |
hardness | Test Condition | Test Method | Test Result |
---|
Rockwell hardness | R-Scale | ASTMD785 | 115 |
flammability | Test Condition | Test Method | Test Result |
---|
UL flame retardant rating | | UL94 | HB |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
| | ASTMD1894 | 0.080 |
Tensile modulus | | ASTMD638 | 2520 MPa |
tensile strength | Yield | ASTMD638 | 55.2到58.6 MPa |
elongation | Break | ASTMD638 | 25到100 % |
Flexural modulus | | ASTMD790 | 2410 MPa |
bending strength | | ASTMD790 | 70.3 MPa |
compressive strength | | ASTMD695 | 72.4 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of cantilever beam gap | | ASTMD256 | 48 J/m |
Electrical performance | Test Condition | Test Method | Test Result |
---|
Volume resistivity | | ASTMD257 | >1.0E+15 ohms·cm |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ASTMD648 | 152 °C |
Continuous use temperature | | 内部方法 | 107 °C |
| | ASTMD3418 | 225 °C |
| | ASTMD696 | 8.6E-05 cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.