PC DX063131 GY7E079L SABIC INNOVATIVE US
32
Form:Granules | Grade:Injection grade
Properties:
Low temperature resistancUV resistanceFiller: Glass fiber reinf30%Filler by weight
Typical Applications:
Electronic and electrical accessoriesAutomotive componentsElectrical enclosureThin walled components
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Electronic and electrical accessories | Automotive components | Electrical enclosure | Thin walled components |
| Properties: | Low temperature resistanc | UV resistance | Filler: Glass fiber reinf | 30% | Filler by weight |
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Dart impact | 23°C,TotalEnergy | ASTM D3763 | 24.0 | J |
| 23°C | ISO 180/1A | 17 | kJ/m² | |
| -30°C | ISO 180/1A | 12 | kJ/m² | |
| 23°C,Natural&BlackColors | ASTM D256 | 190 | J/m | |
| 23°C,Light&WhiteColors | ASTM D256 | 90 | J/m | |
| -30°C | ASTM D256 | 120 | J/m | |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 16 | kJ/m² |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| --1 | ASTM D638 | 7500 | Mpa | |
| Yield, 50.0mm span | ASTM D790 | 170 | Mpa | |
| --6 | ISO 178 | 170 | Mpa | |
| --5 | ISO 178 | 6650 | Mpa | |
| 50.0mm span | ASTM D790 | 7000 | Mpa | |
| crack | ISO 527-2/5 | 3.5 | % | |
| ASTM D638 | 3.6 | % | ||
| ISO 527-2/5 | 90.0 | Mpa | ||
| ASTM D638 | 99.0 | Mpa | ||
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | MD:-40to40°C | ASTME831 | 2.2E-05 | cm/cm/°C |
| 1.8MPa, unannealed, 64.0mm span of | ISO 75-2/Af | 136 | °C | |
| 1.8MPa, unannealed, 3.20mm | ASTM D648 | 136 | °C | |
| Linear coefficient of thermal expansion | TD:-40to40°C | ASTME831 | 6.8E-05 | cm/cm/°C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 0.10 | % |
| Saturation,23°C | ISO 62 | 0.40 | % | |
| Shrinkage rate | MD:3.20mm | Internal Method | 0.30-0.50 | % |
| Melt Volume Flow Rate (MVR) | 300°C/5.0kg | ISO 1133 | 32.0 | cm3/10min |
| melt mass-flow rate | 300°C/5.0kg | ASTM D1238 | 42 | g/10min |
| 300°C/1.2kg | ASTM D1238 | 4.6 | g/10min |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.