Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD792 | 1.44 g/cm³ |
melt mass-flow rate | | ASTMD1238 | 29 g/10min |
Shrinkage rate | | 内部方法 | 0.25到0.70 % |
Water absorption rate | | ASTMD570 | 0.020 % |
density | | ASTMD792 | 1.44 g/cm³ |
melt mass-flow rate | | ASTMD1238 | 29 g/10min |
Shrinkage rate | | 内部方法 | 0.25到0.70 % |
Water absorption rate | | ASTMD570 | 0.020 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
tensile strength | Yield | 内部方法 | 113 MPa |
elongation | Break | 内部方法 | 8.0 % |
elongation | Break | 内部方法 | 8.0 % |
Flexural modulus | | ASTMD790 | 8430 MPa |
bending strength | | ASTMD790 | 157 MPa |
Flexural modulus | | ASTMD790 | 8430 MPa |
bending strength | | ASTMD790 | 157 MPa |
tensile strength | Yield | 内部方法 | 113 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of cantilever beam gap | | ASTMD256 | 88 J/m |
Impact strength of cantilever beam gap | | ASTMD256 | 88 J/m |
Electrical performance | Test Condition | Test Method | Test Result |
---|
Surface Resistivity | | ASTMD257 | 1E+16 ohms |
dielectric strength | | ASTMD149 | 22 kV/mm |
dielectric constant | | ASTMD150 | 3.30 |
dielectric constant | | ASTMD150 | 3.30 |
Surface Resistivity | | ASTMD257 | 1E+16 ohms |
dielectric strength | | ASTMD149 | 22 kV/mm |
dielectric constant | | ASTMD150 | 3.30 |
dielectric constant | | ASTMD150 | 3.30 |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ASTMD648 | 267 °C |
| | ASTMD648 | 267 °C |
| | ASTME831 | 2.5E-5到5.5E-5 cm/cm/°C |
| | ASTME831 | 2.5E-5到5.5E-5 cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.