XLPE Polidan® EC/110

0
  • Properties:
    aging
  • Usages:
    Low voltage insulation
    wire and cable applications

Technical Data Sheet

Test ConditionTest MethodTest Result
Changes in mechanical properties after hot air aging testIEC 6081115 %
Changes in mechanical properties after hot air aging testIEC 60811-8 %
thermosettingIEC 608110.0 %
thermosettingIEC 60811<70 %
Hot air contractionIEC 60811<4.0 %
Volume resistivityIEC 605024.1E+15 ohms·cm
densityASTM D7920.918 g/cm³
melt mass-flow rate内部方法0.70 g/10min
Water absorption rateIEC 60811<0.500 mg/cm²
Water absorption rateIEC 60811<0.500 mg/cm²
Shore hardnessISO 86851
tensile strength BreakIEC 6081121.6 MPa
Bending test variation - in air,IEC 60811无开裂
Volume resistivityIEC 605022.7E+15 ohms·cm
dielectric strengthASTM D14934 kV/mm
dielectric constantASTM D1502.30
Dissipation FactorASTM D1506E-04
dielectric constantIEC 6050215000 Mohms·km
dielectric constantIEC 6050210000 Mohms·km
elongationBreakIEC 60811500 %
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.