PP Osterlene® PPH20NA OSTERMAN USA
Product Description
Certificates(0)
Datasheet
Product Description
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Dart impact | ASTM D5420 | 1.39 | J | |
| Impact strength of cantilever beam gap | 23°C | ASTM D256 | 48 | J/m |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Bending modulus | ASTM D790 | 896 | MPa | |
| elongation | Yield | ASTM D638 | 20 | % |
| tensile strength | Yield | ASTM D638 | 25.5 | MPa |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 0.45MPa,Unannealed | ASTM D648 | 106 | °C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| melt mass-flow rate | 230°C/2.16kg | ASTM D1238 | 20 | g/10min |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Rockwell hardness | R-Scale | ASTM D785 | 108 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.