HDPE TR470UV
0
- Properties:Good impact resistancegood processinggood UV resistancehexene monomerhigh stiffness
- Usages:Pipelinetelecommunications
Technical Data Sheet
processability | Test Condition | Test Method | Test Result |
---|---|---|---|
Melt Temperature | 190-220 ℃ |
Basic performance | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ASTM D-1505 | 0.956 g/cm | |
melt mass-flow rate | ASTM D-1238 | 0.3 g/10min |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Environmental stress cracking | ASTM D-1693B | >100 hr | |
tensile yield strength | ASTM D-638 | 29.4 MPa | |
tensile elongation at break | ASTM D-638 | 600 % | |
Flexural modulus | ASTM D-790 | 1420 MPa | |
IZOD notch impact strength | ASTM D-256 | 294 J/m |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
vicat | ASTM D-1525 | 129 ℃ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.