Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PC K-1300Y TEIJIN JAPAN
PANLITE®
transparent、Translucent accessories、film、sheet、Cleaning Compound
transparent
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Thermal PropertiesTest ConditionTest MethodTEIJIN JAPAN/K-1300Y
Evolution Calendar intelligent importer1.5mmUL746115 °C
Vicat Softening TemperatureASTM D1525/ISO R306151 ℃(℉)
RTIStr1.5mmUL746125 °C
Heat Deflection Temperature1.80MPaISO 75-1132 °C
Flame retardancyUL94HB
Vicat Softening TemperatureISO306/B50151 °C
Linear expansion coefficientASTM D696/ISO 113590.7 mm/mm.℃
Linear thermal expansion coefficientMDISO11359-27E-05 cm/cm/°C
Vicat Softening TemperatureISO 306151 °C
RTIElec1.5mmUL746125 °C
Coefficient of Linear Thermal ExpansionISO 11359-20.7
Heat Deflection Temperature0.45MPa,未退火ISO75-2/B145 °C
1.8MPa,未退火ISO75-2/A132 °C
Linear thermal expansion coefficientTDISO11359-27E-05 cm/cm/°C
Heat Deflection TemperatureASTM D648/ISO 75145 ℃(℉)
Mechanical PropertiesTest ConditionTest MethodTEIJIN JAPAN/K-1300Y
Flexural StrengthASTM D790/ISO 17890 kg/cm²(MPa)[Lb/in²]
Tensile Elongation?(Break)ASTM D638/ISO 527>50 %
Izod Impact Strength带缺口ISO 17989 KJ/m
Tensile ModulusISO 527-12350 Mpa
ISO527-2/12350 Mpa
Nominal Tensile Strain at BreakISO527-2/50>50 %
Flexural ModulusISO 1782200 Mpa
Izod Impact Strength没缺口ISO 179NB KJ/m
Tensile ModulusASTM D638/ISO 5272400 kg/cm²(MPa)[Lb/in²]
Tensile Elongation6 %
Tensile Stress(Yield)ISO 527-160 Mpa
Tensile Elongation断裂>50 %
Flexural ModulusISO1782200 Mpa
Tensile Stress屈服ISO527-2/5060.0 Mpa
Tensile Strain6.0 %
Izod notch impact strengthASTM D256/ISO 17989 kg·cm/cm(J/M)ft·lb/in
Flexural StressISO17890.0 Mpa
Flexural ModulusASTM D790/ISO 1782200 kg/cm²(MPa)[Lb/in²]
Tensile Elongation?(Yield)ISO 527-16 %
PhysicalTest ConditionTest MethodTEIJIN JAPAN/K-1300Y
Melt Volume flow RateISO 11332.5 CM
Moisture Absorption23℃,24hrsISO 620.2 %
Modeling Shrinkage0.5-0.7 %
Melt Volume flow Rate300°C/1.2kgISO11332.80 cm3/10min
Modeling ShrinkageTD:4.00mm内部方法0.50to0.70 %
MD:4.00mm0.50to0.70 %
Moisture Absorption23°C,24hrISO620.20 %
OpticalTest ConditionTest MethodTEIJIN JAPAN/K-1300Y
Index of RefractionASTMD5421.585
Transmittance3mm厚ASTM D100388 %
Index of RefractionASTM D542/ISO 4891.585
TransmittanceASTM D1003/ISO 1346888 %
3000µmASTMD100388.0 %
Physical PropertiesTest ConditionTest MethodTEIJIN JAPAN/K-1300Y
Moisture Absorption 23℃/24HASTM D570/ISO 620.2 %
DensityASTM D792/ISO 11831200
Modeling ShrinkageASTM D9550.5~0.7 %
Impact PropertiesTest ConditionTest MethodTEIJIN JAPAN/K-1300Y
Charpy Unnotched Impact StrengthISO179NoBreak
FlammabilityTest ConditionTest MethodTEIJIN JAPAN/K-1300Y
Flame Rating0.38mmUL94HB
Electrical PropertiesTest ConditionTest MethodTEIJIN JAPAN/K-1300Y
Dielectric StrengthIEC60243-130 KV/mm
Volume ResistivityIEC60093>1.0E+15 ohms·cm
Dielectric Constant-,100HZIEC 602503.1
Comparative Tracking IndexIEC60112250 V
Dissipation Factor?(Tangent)-,100HZIEC 6025010
Arc ResistanceASTM D495/IEC 6011230
Dissipation Factor?(Tangent)-,1MHZIEC 6025090
Dissipation Factor?1MHzIEC602509E-03
Surface ResistivityASTM D257/IEC 60093>1×10 15 Ω
IEC 60093>1×10 Ω
Dielectric ConstantASTM D150/IEC 602503.1
Volume ResistivityASTM D257/IEC 60093>1×10 13 Ω.cm
Surface ResistivityIEC60093>1.0E+15 ohms
Relative Permittivity1MHzIEC602503.00
100Hz3.10
Volume ResistivityIEC 60093>1×10 Ω.m
Dissipation Factor?100HzIEC602501E-03
Dielectric Constant-,1MHzIEC 602503

Contact Us

Get App

Top