Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA+Olefin NEALID XG300 - 8229 AD MAJORIS FRANCE
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | AD MAJORIS FRANCE/NEALID XG300 - 8229 |
|---|---|---|---|
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 200 °C |
| 1.8MPa,Unannealed | ISO 75-2/A | 186 °C | |
| Linear coefficient of thermal expansion | MD | ISO 11359-2 | 2.7E-05 cm/cm/°C |
| Melting temperature | ISO 3146 | 220 °C |
| mechanical properties | Test Condition | Test Method | AD MAJORIS FRANCE/NEALID XG300 - 8229 |
|---|---|---|---|
| Bending modulus | ISO 178 | 7600 MPa | |
| bending strength | ISO 178 | 175 MPa | |
| Tensile modulus | ISO 527-2 | 8500 MPa | |
| Tensile strain | Break | ISO 527-2 | 3.0 % |
| tensile strength | Break | ISO 527-2 | 180 MPa |
| Electrical performance | Test Condition | Test Method | AD MAJORIS FRANCE/NEALID XG300 - 8229 |
|---|---|---|---|
| Compared to the anti leakage trace index | SolutionA | IEC 60112 | PLC 0 |
| Surface resistivity | DIN 53482 | 1E+15 ohms | |
| Volume resistivity | DIN 53482 | 1E+15 ohms·cm |
| Physical properties | Test Condition | Test Method | AD MAJORIS FRANCE/NEALID XG300 - 8229 |
|---|---|---|---|
| density | ISO 1183 | 1.28 g/cm³ | |
| Shrinkage rate | 0.40to0.90 % | ||
| Water absorption rate | Equilibrium,23°C,50%RH | 1.0 % |
| impact performance | Test Condition | Test Method | AD MAJORIS FRANCE/NEALID XG300 - 8229 |
|---|---|---|---|
| Charpy Notched Impact Strength | -20°C | ISO 179/1eA | -- kJ/m² |
| 23°C | ISO 179/1eA | 13 kJ/m² | |
| Impact strength of simply supported beam without notch | -20°C | ISO 179/1eU | -- kJ/m² |
| 23°C | ISO 179/1eU | 41 kJ/m² |
| flammability | Test Condition | Test Method | AD MAJORIS FRANCE/NEALID XG300 - 8229 |
|---|---|---|---|
| Burning wire flammability index | 2.0mm | IEC 60695-2-12 | 650 °C |
| UL flame retardant rating | 1.6mm | UL 94 | HB |