PA66 66IK4 NC DOMO CHEM GERMANY
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

hardnessTest ConditionTest MethodDOMO CHEM GERMANY/66IK4 NC
Rockwell hardnessR -SaleISO 2039-2110
thermal performanceTest ConditionTest MethodDOMO CHEM GERMANY/66IK4 NC
Hot deformation temperature0.45 MPa, UnannealedISO 75-2/B160 °C
1.8 MPa, UnannealedISO 75-2/A65.0 °C
Melting temperatureISO 11357-3262 °C
Vicat softening temperatureISO 306/B50220 °C
mechanical propertiesTest ConditionTest MethodDOMO CHEM GERMANY/66IK4 NC
Bending modulusISO 1781700 Mpa
bending strengthISO 17865.0 Mpa
Tensile modulusISO 527-2/11800 Mpa
Tensile strainBreakISO 527-2/50> 50 %
tensile strengthYieldISO 527-2/5045.0 Mpa
Electrical performanceTest ConditionTest MethodDOMO CHEM GERMANY/66IK4 NC
Surface resistivityIEC 600931.0E+13 ohms
Volume resistivityIEC 600931.0E+15 ohms·cm
Physical propertiesTest ConditionTest MethodDOMO CHEM GERMANY/66IK4 NC
Shrinkage rate横向Flow : 23°C, 72hrISO 25771.6 - 1.8 %
Flow : 23°C, 72hrISO 25771.4 - 1.6 %
Stickiness96% H2SO4ISO 307145 cm³/g
impact performanceTest ConditionTest MethodDOMO CHEM GERMANY/66IK4 NC
Impact strength of simply supported beam without notch-30°CISO 179/1eU无断裂
23°CISO 179/1eU无断裂
Suspended wall beam without notch impact strength23°CISO 180/1U无断裂
flammabilityTest ConditionTest MethodDOMO CHEM GERMANY/66IK4 NC
Burning rateFMVSS 302< 100 mm/min
ISOISO 1874PA66-I.M.14-020
UL flame retardant rating0.8 mmUL 94HB
injectionTest ConditionTest MethodDOMO CHEM GERMANY/66IK4 NC
drying temperature75 to 85 °C
drying time2.0 to 4.0 hr
Mold temperature40 to 80 °C
Processing (melt) temperature270 to 290 °C