Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

EPDM 4640 DOW USA
NORDEL™
chip、container
Toughening
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
physical property | Test Condition | Test Method | DOW USA/4640 |
---|---|---|---|
Transition metal residue | 内部方法 | <10 ppm | |
Ethylene component | ASTM D3900 | 55.0 wt% | |
Ethylene norbornene content | ASTM D6047 | 5.0 wt% | |
Acrylic content | ASTM D3900 | 40.0 wt% | |
molecular weight distribution | 内部方法 | Medium | |
ash content | ASTM D296 | <0.1 wt% | |
Volatile compounds | 内部方法 | <0.40 wt% | |
Mooney viscosity | ML 1+4, 125℃ | ASTM D1646 | 40 MU |