Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPU Multiuse Leostomer® LJ-3190N RIKEN JAPAN
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | RIKEN JAPAN/Multiuse Leostomer® LJ-3190N |
|---|---|---|---|
| Shore hardness | ShoreA,15Sec | ISO 868 | 86 |
| thermal performance | Test Condition | Test Method | RIKEN JAPAN/Multiuse Leostomer® LJ-3190N |
|---|---|---|---|
| Brittle temperature | ISO 974 | -60.0 °C |
| Physical properties | Test Condition | Test Method | RIKEN JAPAN/Multiuse Leostomer® LJ-3190N |
|---|---|---|---|
| density | ISO 1183 | 0.948 g/cm³ | |
| melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 2.5 g/10min |
| aging | Test Condition | Test Method | RIKEN JAPAN/Multiuse Leostomer® LJ-3190N |
|---|---|---|---|
| Change rate of tensile strength in air | 50°C,24hr,在IRM902油中 | ISO 1817 | -11 % |
| Tensile stress change rate | 50°C,24hr,在IRM902油中,Break | ISO 1817 | 9.0 % |
| elastomer | Test Condition | Test Method | RIKEN JAPAN/Multiuse Leostomer® LJ-3190N |
|---|---|---|---|
| elongation | Break | ISO 37 | 920 % |
| Permanent compression deformation | -- | ISO 815 | 57 % |
| 70°C,22hr | ISO 815 | 50 % | |
| tear strength | ISO 34-1 | 67 kN/m | |
| tensile strength | 100%Strain | ISO 37 | 4.80 MPa |
| Yield | ISO 37 | 20.0 MPa |