TPU-Ether Jamplast JPTPUET Jamplast, Inc.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | Jamplast, Inc./Jamplast JPTPUET |
---|---|---|---|
Shore hardness | 邵氏A | ASTM D2240 | 86 |
Mechanical properties | Test Condition | Test Method | Jamplast, Inc./Jamplast JPTPUET |
---|---|---|---|
Taber abraser | 1000Cycles,1000g,H-22转轮 | ASTM D1044 | 50.0 mg |
physical property | Test Condition | Test Method | Jamplast, Inc./Jamplast JPTPUET |
---|---|---|---|
Shrinkage rate | TD:1.60mm | ASTM D955 | 0.50to0.60 % |
density | ASTM D792 | 1.18 g/cm³ | |
melt mass-flow rate | 224°C/1.2kg | ASTM D1238 | 35 g/10min |
Shrinkage rate | MD:1.60mm | ASTM D955 | 0.50to0.60 % |
elastomer | Test Condition | Test Method | Jamplast, Inc./Jamplast JPTPUET |
---|---|---|---|
elongation | 断裂 | ASTM D412 | 530 % |
tensile strength | 断裂 | ASTM D412 | 40.3 MPa |
50%应变 | ASTM D412 | 5.86 MPa | |
100%应变 | ASTM D412 | 7.24 MPa | |
300%应变 | ASTM D412 | 15.2 MPa | |
tear strength | ASTM D624 | 91.1 kN/m | |
compression set | 25°C,22hr | ASTM D395 | 25 % |
Thermal performance | Test Condition | Test Method | Jamplast, Inc./Jamplast JPTPUET |
---|---|---|---|
vicat | ASTM D1525 | 92.2 °C | |
Glass Transition Temperature | DSC | -37.2 °C | |
Linear coefficient of thermal expansion | MD | ASTM D696 | 1.5E-04 cm/cm/°C |