Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

POM TG-61 KEP KOREA
KEPITAL®
--
Wear resistance,High rigidity
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
thermal performance | Test Condition | Test Method | KEP KOREA/TG-61 |
---|---|---|---|
1.8MPa, unannealed | ASTM D648 | 164 °C | |
ISO 75-2/A | 163 °C | ||
Linear coefficient of thermal expansion | MD:20到80°C | ASTM D696 | 1.3E-04 cm/cm/°C |
Melting temperature | ASTM D3418 | 165 °C |
mechanical properties | Test Condition | Test Method | KEP KOREA/TG-61 |
---|---|---|---|
23°C | ASTM D790 | 201 Mpa | |
ISO 178 | 240 Mpa | ||
Fracture, 23 ° C | ASTM D638 | 3.0 % | |
ISO 527-2 | 2.0 % | ||
Surrender, 23 ° C | ASTM D638 | 147 Mpa | |
ISO 527-2 | 170 Mpa |
Electrical performance | Test Condition | Test Method | KEP KOREA/TG-61 |
---|---|---|---|
Surface resistivity | ASTMD257 | 1E+16 ohms | |
Volume resistivity | ASTMD257 | 1E+14 ohms·cm |
Physical properties | Test Condition | Test Method | KEP KOREA/TG-61 |
---|---|---|---|
2.00mm | ASTM D955 | 0.50 % | |
190°C/2.16kg | ASTM D1238 | 5.0 g/10min | |
3.00mm | 3.00mm | ISO 294-4 | 0.20 % |
Water absorption rate | 平衡,23°C,60%RH | ASTM D570 | 0.20 % |
impact performance | Test Condition | Test Method | KEP KOREA/TG-61 |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179/1eA | 10 kJ/m² | |
Impact strength of cantilever beam gap | 3.20mm | ASTM D256 | 78 J/m |
flammability | Test Condition | Test Method | KEP KOREA/TG-61 |
---|---|---|---|
UL flame retardant rating | 0.800mm | UL 94 | HB |