| thermal performance | Test Condition | Test Method | Samsung Cheil South Korea/UT-0520I |
|---|---|---|---|
| Vicat softening temperature | ISO R 306 | 90 °C | |
| Hot deformation temperature | 264psi Unannealed,0.250in | ASTM-D648 | 80 °C |
| Obstructive performance | 0.0591 in | UL 94 | HB |
| Physical properties | Test Condition | Test Method | Samsung Cheil South Korea/UT-0520I |
| Shrinkage rate | ASTM-D955 | 0.3-0.7 % | |
| density | ASTM-D792 | 1.08 | |
| mechanical properties | Test Condition | Test Method | Samsung Cheil South Korea/UT-0520I |
| bending strength | ASTM-D790 | 53.9 Mpa | |
| tensile strength | ASTM-D638 | 38.9 Mpa | |
| Bending modulus | ASTM-D790 | 1798.2 Mpa | |
| Impact strength of cantilever beam gap | 23℃,0.125in | ASTM-D256 | 3.67 ft-1b/in |
| Rockwell hardness | ASTM-D785 | 100 R-Scale | |
| Basic Performance | Test Condition | Test Method | Samsung Cheil South Korea/UT-0520I |
| melt mass-flow rate | 220℃/10kg | ASTM-D1238 | 12 g/10min |