Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PP OMIKRON FMS 30 R NERO 808 TECNOPOL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | TECNOPOL/OMIKRON FMS 30 R NERO 808 |
---|---|---|---|
Impact strength of cantilever beam gap | 23°C | ISO 180 | 14 kJ/m² |
0°C | ISO 180 | 7.5 kJ/m² |
Mechanical properties | Test Condition | Test Method | TECNOPOL/OMIKRON FMS 30 R NERO 808 |
---|---|---|---|
Tensile strain | 断裂 | ISO 527-2 | 40 % |
tensile strength | 屈服 | ISO 527-2 | 20.0 MPa |
Flexural modulus | ISO 178 | 1700 MPa |
flammability | Test Condition | Test Method | TECNOPOL/OMIKRON FMS 30 R NERO 808 |
---|---|---|---|
burning rate | FMVSS302 | <100 mm/min | |
UL flame retardant rating | UL 94 | HB |
physical property | Test Condition | Test Method | TECNOPOL/OMIKRON FMS 30 R NERO 808 |
---|---|---|---|
density | ISO 1183 | 1.00 g/cm³ | |
melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 9.0 g/10min |
aging | Test Condition | Test Method | TECNOPOL/OMIKRON FMS 30 R NERO 808 |
---|---|---|---|
Accelerated aging | 150°C | 内部方法 | 6.3 day |
Thermal performance | Test Condition | Test Method | TECNOPOL/OMIKRON FMS 30 R NERO 808 |
---|---|---|---|
vicat | ISO 306/B | 55.0 °C | |
Heat distortion temperature | 1.8MPa,未退火,HDT | ISO 75-2/A | 53.0 °C |
Contact Us
Get App
Top