Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PEEK 1330 Arlon-MED
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | Arlon-MED/1330 |
---|---|---|---|
Suspended wall beam without notch impact strength | ASTM D256 | 1000 J/m | |
Impact strength of cantilever beam gap | ASTM D256 | 57 J/m |
hardness | Test Condition | Test Method | Arlon-MED/1330 |
---|---|---|---|
Shore hardness | 邵氏D | ASTM D2240 | 85 |
Mechanical properties | Test Condition | Test Method | Arlon-MED/1330 |
---|---|---|---|
shear strength | 232°C | ASTM D732 | 19.8 MPa |
elongation | 断裂 | ASTM D638 | 20 % |
compressive strength | ASTM D695 | 107 MPa | |
coefficient of friction | ASTM D1894 | 0.15 | |
tensile strength | 断裂 | ASTM D638 | 86.9 MPa |
Flexural modulus | ASTM D790 | 3690 MPa | |
bending strength | ASTM D790 | 145 MPa | |
Wear factor | ASTM D3702 | 40 10^-8mm³/N·m | |
shear strength | 23°C | ASTM D732 | 77.6 MPa |
physical property | Test Condition | Test Method | Arlon-MED/1330 |
---|---|---|---|
Water absorption rate | 24hr | ASTM D570 | 0.35 % |
density | ASTM D792 | 1.37 g/cm³ |
Thermal performance | Test Condition | Test Method | Arlon-MED/1330 |
---|---|---|---|
Heat distortion temperature | 1.8MPa,未退火,HDT | ASTM D648 | 166 °C |
Linear coefficient of thermal expansion | MD:>149°C | ASTM D696 | 1.5E-04 cm/cm/°C |
MD:<149°C | ASTM D696 | 4.1E-05 cm/cm/°C | |
melting temperature | 343 °C |