Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PC+TPU 80A DSM Additive Manufacturing
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | DSM Additive Manufacturing/ 80A |
---|---|---|---|
Shore hardness | 邵氏A | ASTM D2240 | 83 |
Mechanical properties | Test Condition | Test Method | DSM Additive Manufacturing/ 80A |
---|---|---|---|
Taber abraser | 1000Cycles,1000g,H-18转轮 | ASTM D1044 | 5.70 mg |
tensile strength | 极限 | ASTM D638 | 46.6 MPa |
300%应变 | ASTM D638 | 16.9 MPa | |
elongation | 断裂 | ASTM D638 | 530 % |
tensile strength | 100%应变 | ASTM D638 | 6.01 MPa |
coefficient of friction | 与自身-动态 | ASTM D1894 | 1.5 |
tensile strength | 50%应变 | ASTM D638 | 4.37 MPa |
Flexural modulus | ASTM D790 | 28.7 MPa | |
bending strength | 5.0%应变 | ASTM D790 | 1.24 MPa |
Electrical performance | Test Condition | Test Method | DSM Additive Manufacturing/ 80A |
---|---|---|---|
dielectric constant | 60Hz | ASTM D150 | 5.00 |
dielectric strength | ASTM D149 | 17 kV/mm |
physical property | Test Condition | Test Method | DSM Additive Manufacturing/ 80A |
---|---|---|---|
Water absorption rate | 饱和 | ASTM D570 | 1.2 % |
density | ASTM D792 | 1.19 g/cm³ | |
melt mass-flow rate | 224°C/1.2kg | ASTM D1238 | 22 g/10min |
Shrinkage rate | MD:--3 | ASTM D955 | 1.2 % |
MD:--2 | ASTM D955 | 0.0to3.0 % |
elastomer | Test Condition | Test Method | DSM Additive Manufacturing/ 80A |
---|---|---|---|
tear strength | ASTM D624 | 64.8 kN/m |
Thermal performance | Test Condition | Test Method | DSM Additive Manufacturing/ 80A |
---|---|---|---|
vicat | ASTM D1525 | 78.3 °C | |
Linear coefficient of thermal expansion | MD | ASTME831 | 1.6E-04 cm/cm/°C |
Contact Us
Get App
Top