Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

Propylene Elastomer Vistamaxx™ 6202FL ExxonMobil
--
Packaging, film, composite
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | ExxonMobil/Vistamaxx™ 6202FL |
|---|---|---|---|
| Shore hardness | ShoreA | ASTM D2240 | 66 |
| mechanical properties | Test Condition | Test Method | ExxonMobil/Vistamaxx™ 6202FL |
|---|---|---|---|
| Bending modulus | ASTM D790 | 12.3 MPa | |
| elongation | Break | ASTM D638 | >2000 % |
| tensile strength | 100%Strain | ASTM D638 | 1.93 MPa |
| 300%Strain | ASTM D638 | 2.10 MPa | |
| Break | ASTM D638 | >5.50 MPa |
| Physical properties | Test Condition | Test Method | ExxonMobil/Vistamaxx™ 6202FL |
|---|---|---|---|
| density | ASTM D1505 | 0.863 g/cm³ | |
| melt mass-flow rate | 190°C/2.16kg | ASTM D1238 | 9.1 g/10min |
| elastomer | Test Condition | Test Method | ExxonMobil/Vistamaxx™ 6202FL |
|---|---|---|---|
| tear strength | ASTM D624 | 33.3 kN/m |