PC Iupilon® GSH2010PH Mitsubishi Chemical Corporation
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | Mitsubishi Chemical Corporation/Iupilon® GSH2010PH |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO 179 | 10 kJ/m² |
Impact strength of simply supported beam without notch | 23°C | ISO 179 | NoBreak |
Electrical performance | Test Condition | Test Method | Mitsubishi Chemical Corporation/Iupilon® GSH2010PH |
---|---|---|---|
Compared to the Leakage Tracking Index (CTI) | CTI | UL 746 | PLC 3 |
Mechanical properties | Test Condition | Test Method | Mitsubishi Chemical Corporation/Iupilon® GSH2010PH |
---|---|---|---|
Nominal tensile fracture strain | ISO 527-2 | 10 % | |
Tensile modulus | ISO 527-2 | 2900 MPa | |
Tensile strain | 屈服 | ISO 527-2 | 5.0 % |
tensile strength | 屈服 | ISO 527-2 | 52.0 MPa |
Flexural modulus | ISO 178 | 2700 MPa | |
bending strength | ISO 178 | 90.0 MPa |
flammability | Test Condition | Test Method | Mitsubishi Chemical Corporation/Iupilon® GSH2010PH |
---|---|---|---|
UL flame retardant rating | 0.40mm | UL 94 | HB |
physical property | Test Condition | Test Method | Mitsubishi Chemical Corporation/Iupilon® GSH2010PH |
---|---|---|---|
Shrinkage rate | TD:3.20mm | 0.30to0.50 % | |
吸水率(饱和,23°C) | 0.14 % | ||
Melt volume flow rate | 300°C/1.2kg | ISO 1133 | 14.0 cm³/10min |
Shrinkage rate | MD:3.20mm | 0.30to0.50 % | |
density | ISO 1183 | 1.26 g/cm³ | |
melt mass-flow rate | 300°C/1.2kg | ISO 1133 | 15 g/10min |
Thermal performance | Test Condition | Test Method | Mitsubishi Chemical Corporation/Iupilon® GSH2010PH |
---|---|---|---|
Heat distortion temperature | 0.45MPa,未退火,HDT | ISO 75-2/B | 132 °C |
1.8MPa,未退火,HDT | ISO 75-2/A | 125 °C | |
Linear coefficient of thermal expansion | MD | ISO 11359-2 | 5.8E-05 cm/cm/°C |
TD | ISO 11359-2 | 5.8E-05 cm/cm/°C |