PA6 R250-H/HGK/GF 20/10 ALMAAK GERMANY
--
--
Filler, glass fiber reinforced material, 10%, filler by weight, glass beads, 20%, filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | ALMAAK GERMANY/ R250-H/HGK/GF 20/10 |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 3.5 kJ/m² |
Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 25 kJ/m² |
Mechanical properties | Test Condition | Test Method | ALMAAK GERMANY/ R250-H/HGK/GF 20/10 |
---|---|---|---|
tensile strength | 断裂 | ISO 527-2/5 | 75.0 MPa |
Tensile strain | 断裂 | ISO 527-2/5 | 1.5 % |
Tensile modulus | ISO 527-2/1 | 5500 MPa |
flammability | Test Condition | Test Method | ALMAAK GERMANY/ R250-H/HGK/GF 20/10 |
---|---|---|---|
UL flame retardant rating | 1.6mm | UL 94 | HB |
physical property | Test Condition | Test Method | ALMAAK GERMANY/ R250-H/HGK/GF 20/10 |
---|---|---|---|
density | 23°C | ISO 1183 | 1.03 g/cm³ |
Shrinkage rate | TD | ISO 294-4 | 0.50 % |
MD | ISO 294-4 | 0.30 % |
Thermal performance | Test Condition | Test Method | ALMAAK GERMANY/ R250-H/HGK/GF 20/10 |
---|---|---|---|
vicat | ISO 306/B50 | 205 °C | |
Heat distortion temperature | 1.8MPa,未退火,HDT | ISO 75-2/A | 180 °C |
melting temperature | DSC | 220 °C |