| injection | Test Condition | Test Method | OPP OMAN/HP2106N |
|---|---|---|---|
| Mold temperature | 20 to 40 °C | ||
| Injection speed | 快速 | ||
| Processing (melt) temperature | 220 to 260 °C | ||
| Maintain pressure | 20.0 to 50.0 Mpa | ||
| mechanical properties | Test Condition | Test Method | OPP OMAN/HP2106N |
| tensile strength | Yield | ISO 527-2/50 | 34 Mpa |
| Tensile strain | Yield | 9 % | |
| Tensile modulus | ISO 527-1/1 | 1550 Mpa | |
| Tensile strain | Break | > 50 % | |
| thermal performance | Test Condition | Test Method | OPP OMAN/HP2106N |
| Hot deformation temperature | 0.45 MPa, Unannealed | ISO 75-2/B | 85 °C |
| Vicat softening temperature | ISO 306 | 153 °C | |
| Physical properties | Test Condition | Test Method | OPP OMAN/HP2106N |
| melt mass-flow rate | 230°C/2.16 kg | ISO 1133 | 12 g/10 min |