Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PP HP2106N OPP OMAN
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
thermal performance | Test Condition | Test Method | OPP OMAN/HP2106N |
---|---|---|---|
Hot deformation temperature | 0.45 MPa, Unannealed | ISO 75-2/B | 85 °C |
Vicat softening temperature | ISO 306 | 153 °C |
mechanical properties | Test Condition | Test Method | OPP OMAN/HP2106N |
---|---|---|---|
Tensile modulus | ISO 527-1/1 | 1550 Mpa | |
Tensile strain | Yield | 9 % | |
Break | > 50 % | ||
tensile strength | Yield | ISO 527-2/50 | 34 Mpa |
Physical properties | Test Condition | Test Method | OPP OMAN/HP2106N |
---|---|---|---|
melt mass-flow rate | 230°C/2.16 kg | ISO 1133 | 12 g/10 min |
injection | Test Condition | Test Method | OPP OMAN/HP2106N |
---|---|---|---|
Injection speed | 快速 | ||
Maintain pressure | 20.0 to 50.0 Mpa | ||
Mold temperature | 20 to 40 °C | ||
Processing (melt) temperature | 220 to 260 °C |