PPO/PA GTX810-71167 SABIC INNOVATIVE US
NORYL GTX™ 
Casters,fibre
Chemical resistance,enhance,High temperature resistan
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

hardnessTest ConditionTest MethodSABIC INNOVATIVE US/GTX810-71167
Rockwell hardnessR-ScaleASTM D785119
thermal performanceTest ConditionTest MethodSABIC INNOVATIVE US/GTX810-71167
Hot deformation temperature0.45 MPa, Unannealed, 6.40 mmASTM D648245 °C
1.8 MPa, Unannealed, 6.40 mmASTM D648210 °C
Linear coefficient of thermal expansion-20 to 150°C,FlowASTM E8314.0E-5 - 5.0E-5 cm/cm/°C
RTIUL 74650.0 °C
RTI ElecUL 74650.0 °C
RTI ImpUL 74650.0 °C
Vicat softening temperatureASTM D15253240 °C
mechanical propertiesTest ConditionTest MethodSABIC INNOVATIVE US/GTX810-71167
Bending modulus100 mm SpanASTM D7903960 Mpa
bending strengthYield, 100 mm SpanASTM D790155 Mpa
elongationBreakASTM D63810 %
tensile strengthYieldASTM D63889.0 Mpa
BreakASTM D63888.0 Mpa
Electrical performanceTest ConditionTest MethodSABIC INNOVATIVE US/GTX810-71167
Arc resistanceASTM D495PLC 6
Compared to the anti leakage trace indexUL 746PLC 3
High arc combustion indexUL 746PLC 0
High voltage arc tracing rateUL 746PLC 3
Hot wire ignitionUL 746PLC 0
Physical propertiesTest ConditionTest MethodSABIC INNOVATIVE US/GTX810-71167
Shrinkage rateAcross FlowFlow : 3.20 mmInternal Method0.65 - 0.85 %
Flow : 3.20 mmInternal Method0.60 - 0.80 %
Water absorption rate24 hr, 50% RHASTM D5700.50 %
Equilibrium, 50% RHASTM D5701.0 %
flammabilityTest ConditionTest MethodSABIC INNOVATIVE US/GTX810-71167
UL flame retardant rating1.5 mmUL 94HB
injectionTest ConditionTest MethodSABIC INNOVATIVE US/GTX810-71167
Back pressure0.300 to 1.40 Mpa
drying temperature95 to 105 °C
drying time3.0 to 4.0 hr
Exhaust hole depth0.013 to 0.038 mm
Mold temperature75 to 120 °C
Processing (melt) temperature280 to 305 °C
Screw speed20 to 100 rpm
Spray nozzle temperature280 to 305 °C
Suggested injection volume30 to 50 %
Suggested maximum moisture content0.070 %
Temperature at the front of the material cylinder275 to 305 °C
Temperature at the rear of the barrel265 to 305 °C
Temperature in the middle of the barrel270 to 305 °C