TPO K PP 7200 Technovinyl Polymers India Ltd.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodTechnovinyl Polymers India Ltd./K PP 7200
Impact strength of cantilever beam gap23°CASTM D256>120 J/m
Supplementary InformationTest ConditionTest MethodTechnovinyl Polymers India Ltd./K PP 7200
HeatResistance-ElevatedTemp100°CNochangeinshapeorsurface
Mechanical propertiesTest ConditionTest MethodTechnovinyl Polymers India Ltd./K PP 7200
Flexural modulusASTM D790>1500 MPa
scratch resistance内部方法<2.00 dL
tensile strength 屈服ASTM D638>19.0 MPa
physical property Test ConditionTest MethodTechnovinyl Polymers India Ltd./K PP 7200
LightFastnessSAEJ18852 month
Shrinkage rateMD<1.1 %
melt mass-flow rate230°C/2.16kgASTM D1238>14 g/10min
densityASTM D7920.980to1.02 g/cm³
agingTest ConditionTest MethodTechnovinyl Polymers India Ltd./K PP 7200
thermal ageing150°C,高温NodecompositiontypicalofPP
Thermal performanceTest ConditionTest MethodTechnovinyl Polymers India Ltd./K PP 7200
Heat distortion temperature0.45MPa,未退火,HDTASTM D648>130 °C