Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

LDPE CA4676 Cabot Corporation
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | Cabot Corporation/ CA4676 |
|---|---|---|---|
| Shore hardness | ShoreD | ASTM D2240 | 50 |
| mechanical properties | Test Condition | Test Method | Cabot Corporation/ CA4676 |
|---|---|---|---|
| Tensile strain | Break,3.00mm | ISO 527-2 | 390 % |
| tensile strength | Yield,3.00mm | ISO 527-2 | 11.0 MPa |
| Break,3.00mm | ISO 527-2 | 13.0 MPa |
| Electrical performance | Test Condition | Test Method | Cabot Corporation/ CA4676 |
|---|---|---|---|
| Surface resistivity | 0.100mm | Internal Method | 2.5E+04 ohms |
| Volume resistivity | 4.00mm | Internal Method | 10 ohms·cm |
| Physical properties | Test Condition | Test Method | Cabot Corporation/ CA4676 |
|---|---|---|---|
| density | 23°C | Internal Method | 0.990 g/cm³ |
| melt mass-flow rate | 190°C/5.0kg | ISO 1133 | 0.90 g/10min |
| 190°C/21.6kg | ISO 1133 | 29 g/10min | |
| 190°C/10.0kg | ISO 1133 | 4.8 g/10min |