PUR-Capro Vibrathane® 8030 CHEMTURU USA
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | CHEMTURU USA/Vibrathane® 8030 |
|---|---|---|---|
| Shore hardness | ShoreA | ASTM D2240 | 80 |
| thermosetting | Test Condition | Test Method | CHEMTURU USA/Vibrathane® 8030 |
|---|---|---|---|
| Post curing time | 115°C | 16 hr | |
| storage stability | 5.0 min |
| Uncured Properties | Test Condition | Test Method | CHEMTURU USA/Vibrathane® 8030 |
|---|---|---|---|
| Curing time | 115°C | 0.50 hr |
| elastomer | Test Condition | Test Method | CHEMTURU USA/Vibrathane® 8030 |
|---|---|---|---|
| elongation | Break | ASTM D412 | 300 % |
| Permanent compression deformation | 70°C,22hr | ASTM D395B | 29 % |
| tear strength | Split | ASTM D470 | 21 kN/m |
| tensile strength | ASTM D412 | 33.1 MPa | |
| 100%Strain | ASTM D412 | 4.83 MPa |