IIR SIBUR Synthetic Rubber BK-1675N / IIR-1675 SIBUR RUSSIA
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Physical propertiesTest ConditionTest MethodSIBUR RUSSIA/SIBUR Synthetic Rubber BK-1675N / IIR-1675
ash contentASTM D5667<0.40 %
Calcium StearateInternal Method<1.2 %
Mooney viscosityML1+8,125°CASTM D164646to56 MU
UnsaturationInternal Method1.40to1.80 mol%
Volatile compoundsASTM D5668<0.30 %
elastomerTest ConditionTest MethodSIBUR RUSSIA/SIBUR Synthetic Rubber BK-1675N / IIR-1675
elongationBreakASTM D412>450 %
tensile strength300%StrainASTM D412>6.00 MPa
YieldASTM D412>13.0 MPa