Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
ABS Novodur® P2HGV INEOS Barex
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodINEOS Barex/Novodur® P2HGV
Charpy Notched Impact Strength23°CISO 1796.0 kJ/m²
-30°CISO 1795.0 kJ/m²
Impact strength of simply supported beam without notch-30°CISO 17920 kJ/m²
23°CISO 17918 kJ/m²
Impact strength of cantilever beam gap23°CISO 180/A7.0 kJ/m²
-30°CISO 180/A5.0 kJ/m²
hardnessTest ConditionTest MethodINEOS Barex/Novodur® P2HGV
ball-indentation hardnessISO 2039-1135 MPa
Electrical performanceTest ConditionTest MethodINEOS Barex/Novodur® P2HGV
Compared to the Leakage Tracking Index (CTI)IEC 60112PLC 1
Volume resistivityIEC 60093>1.0E+15 ohms·cm
relative permittivity100HzIEC 602502.90
Dissipation Factor100HzIEC 602505E-03
relative permittivity1MHzIEC 602503.10
Surface ResistivityIEC 600931E+14 ohms
dielectric strength1.50mmIEC 60243-132 kV/mm
Dissipation Factor1MHzIEC 602506E-03
Mechanical propertiesTest ConditionTest MethodINEOS Barex/Novodur® P2HGV
Tensile strain断裂,23°CISO 527-22.0 %
tensile strength 屈服,23°CISO 527-274.0 MPa
Tensile modulusISO 527-25500 MPa
tensile strength 断裂,23°CISO 527-274.0 MPa
Flexural modulusISO 1785400 MPa
bending strengthISO 178101 MPa
physical property Test ConditionTest MethodINEOS Barex/Novodur® P2HGV
Melt volume flow rate220°C/10.0kgISO 11333.00 cm³/10min
ash content16 %
Shrinkage rateISO 294-40.20to0.40 %
densityISO 11831.16 g/cm³
Thermal performanceTest ConditionTest MethodINEOS Barex/Novodur® P2HGV
Heat distortion temperature1.8MPa,退火,HDTISO 75-2/A102 °C
vicatISO 306/B50105 °C
Heat distortion temperature0.45MPa,退火,HDTISO 75-2/B106 °C
Linear coefficient of thermal expansionMDISO 11359-14E-05 cm/cm/°C

Contact Us

Get App

Top